| Sign In | Join Free | My polstate.com |
|
Brand Name : GH3600
Certification : COO, CCPIT
Place of Origin : China
MOQ : 50 kgs
Price : negotiation
Payment Terms : Ex works/ FOB/ CPT
Supply Ability : 30,000 kgs/ month
Delivery Time : 25-30 days
Packaging Details : Wooden box
Condition : Bright/ Oxidized Soft/ Hard
Surface : Bright
Diameter : 3-50mm
Shape : Strip, Foil, Sheet, Wire, Bar.
Name : Inconel 600 UNS N06600 GH3600
High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator
Quick Detail:
| Name | Inconel 600 UNS N06600 GH3600
| Application | thermowell work in Erosion atmosphere; Anti-chlorine, hydrogen chloride, oxidation and carbonization corrosion; Nuclear reactor |
| Condition | Bright/ Oxidized Soft/ Hard | Feature | GH3600 for a variety of corrosive media have corrosion resistance. Petrochemical production of catalytic regenerator over 700 ℃ applications alloy 600 is recommended for longer life. |
| Shape | Strip, Foil, Sheet, Wire, Bar. | Standard |
|
Description:
Physical properties
>Density (g/cm3): 8.4
>Melting point (℃): 1370~1425
Chemical composition(%)
| Grade | C | Si | Mn | P | S | Ni | Cr | Cu | Fe |
| GH3600 | ≤0.15 | ≤0.5 | ≤ 1 | ≤0.015 | ≤0.015 | 72 | 14~17 | ≤0.5 | 6~7 |
Mechanical properties
|
|
| Yield Strength (Mpa) | Tensile Strength (Mpa) | Elongation, % | Hardness, HB |
| GH3600 | Cold-rolling | 240 | 550 | 30 | ≤195 |
| As annealed | 180 | 500 | 35 | ≤185 |
Specifications
| Grade | GH3600 |
| Size | Ф 3~50mm |
| MOQ | 50 kgs |
| Condition | Soft/ Hard; Bright/ Oxidized |